1The initial volume fraction of retained austenite (*f*g0) and its carbon concentration (*C*g0) increase in steel B due to the combined addition of Al-Nb-Mo.
“Both *f*g0 and *C*g0 are increased by combined addition of Al-Nb-Mo.”