Applied Science · youtube · en-US
1The copper plating process requires dipping the part in a catalyst, then washing it, and finally immersing it in a magic solution to deposit copper.
“and so the basic process is to really wash this really well dip it in the catalyst wash it again and then dip it into the magic solution and take it out and you'll have a copper part”
spoken · 205s · 2018-09-03
Applied Science · youtube · en-US
2The magic solution is unstable and typically lasts only one to two days due to its reactive nature.
“this solution here will probably not last more than a day or two I've experimented with different formulations”