Tm doping

4 moment(s) that assert this concept — showing 1–4 of 4

single sourceRests on a single channel — treat as a lead, verify independently
↣ how this spread over time →
provenance — click a node to open its encoding unit
[1] Simón[2] Simón[3] Simón[4] Simón
showing 4 of 4 moments
scholarly papers (1)
Simón Rivier · openalex · zh
1Tm³⁺-doped monoclinic double tungstates have an absorption line centered near 800 nm with a broad longwave wing, making them ideal for room-temperature pumping with commercial AlGaAs laser diodes.
“In the case of Tm 3+ -doping, an additional advantage is that the absorption line is centered near 800 nm [9] with a broader longwave wing”
written · p. 3 · 2007-01-01
Simón Rivier · openalex · zh
2Efficient continuous-wave laser operation around 2 µm was achieved in Tm-doped KGdW and KLuW crystals.
“Efficient CW laser operation around 2 µm was also achieved in Tm-doped KGdW [15] and KLuW [16]”
written · p. 3 · 2007-01-01
Simón Rivier · openalex · zh
3Liquid phase epitaxy using K₂W₂O₇ solvent produces high-quality Tm:KYW waveguide layers with thicknesses up to 40 µm and Tm concentrations from 0.7 to 1.2 at% at a growth rate of 18 µm/h.
“LPE is a well-known technique for the production of high-quality oxide films for laser applications, in which a single-crystal layer can be grown from a molten solution on a flat, oriented single-crystal substrate. 1-mm thick undoped KYW crystals with laser-grade polished (010) faces were used as substrates. The vertical dipping technique with partial immersion of the substrate was applied. Out of the two solvents employed recently for the fabrication of rare-earth-ion-doped KYW waveguides, a low-temperature chloride solvent [20] or K₂W₂O₇ [21], we chose the latter because of the much better interface and layer quality obtained with K₂W₂O₇ [19]. Single-crystalline layers with thickness up to 40 µm and different Tm 3+ concentrations ranging from 0.7 to 1.2at% were obtained at a growth rate of 18 µm/h”
written · p. 4 · 2007-01-01
Simón Rivier · openalex · zh
4The refractive index of Tm:KYW increases linearly with Tm concentration, with a measured increase of 6×10⁻⁴ in a 1.8 at% Yb-doped layer compared to undoped KYW.
“Since KTmW is isostructural to KYW, the refractive indices of Tm:KYW layers increase approximately linearly with increasing Tm concentration. In a thin KYW layer doped with 1.8at% Yb, we measured a refractive-index increase of 6x10 -4 compared to the undoped KYW substrate by dark m-lines spectroscopy [19]”
written · p. 4 · 2007-01-01